● Low repair method:
Equipment: with automatic temperature control, timing, and more specifications of the tubular cavity pressure equipment.
Rubber: agree with filling wire by wire, and gel content than be fill material, slightly stronger vulcanization system.
Three, operation method:
1, according to the set temperature and time of rubber vulcanization system
2, wash with rubber ink thinner, polishing the repair, especially attaches to fully process.
3, according to the size of the gap in the proper amount of shearing repair adhesive material, pay attention to not more or less,
4, good cut rubber plug the gaps, pay attention to the rubber circumferential surface not higher than the wire.
5, wrapped in high temperature resistant PP belt. And put it in a slightly smaller than the line diameter of the tubular cavity, lock up and die, let the position has certain pressure. Pay attention to the cavity diameter slightly smaller than wire diameter 0.1 ~ 0.2 mm.
6, curing time, take out the products, if you have a small amount of rubber overflow, as with a sharp blade, and with thinner polishing to do.
Four, validation methods:
To press the right amount of air into the wire and placed in the water, see any leakage phenomenon can be judged good or bad.